Pull-Off Test For Carbon Fiber Laminate Systems

Pull-Off Test For Carbon Fiber Laminate Systems Based on ACI

Pull-Off Test For Carbon Fiber Laminate Systems


According to ACI 440.2R-17 (Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures), the Pull-off Test for carbon fiber reinforced polymer (CFRP) plates is a critical method for evaluating the bond performance between CFRP plates and substrates (e.g., concrete). Below are the criteria for success and failure:



1. Successful Pull-off Test Result: Cohesive Failure

  • Definition: During the pull-off test, failure occurs within the concrete substrate (i.e., the concrete itself fractures), rather than at the bond interface between the CFRP plate and the concrete.

  • Significance:

    • Indicates that the bond strength is higher than the tensile strength of the concrete itself, which is the ideal outcome.

    • Demonstrates excellent bond performance between the CFRP plate and the concrete, ensuring the CFRP plate can fully deliver its strengthening effect.

  • ACI Standard: Cohesive failure is the preferred criterion for judging bond performance as acceptable.


2. Failed Pull-off Test Result: Adhesive Failure

  • Definition: During the pull-off test, failure occurs at the bond interface between the CFRP plate and the concrete, meaning the CFRP plate detaches from the concrete surface.

  • Significance:

    • Indicates insufficient bond strength, which may be due to improper surface preparation, unsuitable adhesive selection, or construction issues.

    • This failure mode suggests that the CFRP plate cannot fully utilize its strengthening potential, potentially compromising the structure's safety and durability.

  • ACI Standard: Adhesive failure is generally considered unacceptable, requiring reevaluation of construction techniques or material selection.


3. Other Possible Failure Modes

  • Mixed Failure: Partial failure occurs within the concrete, and partial failure occurs at the bond interface.

    • ACI considers this failure mode as intermediate, requiring further analysis to determine the root cause.

  • FRP Rupture: If the CFRP plate fractures during the pull-off test, it indicates that the bond strength exceeds the tensile strength of the CFRP plate itself.

    • Although rare, this scenario also demonstrates excellent bond performance.


4. ACI Requirements for Pull-off Tests

  • Testing Frequency: ACI recommends random sampling during construction to ensure consistent bond quality.

  • Minimum Strength Requirement: The bond strength must meet the design value, and the failure mode should be cohesive failure.

  • Surface Preparation: ACI emphasizes the importance of concrete surface cleanliness, roughness, and moisture control for optimal bond performance.


ผลิตภัณฑ์ที่แนะนำโดย Horse Construction

คุณสามารถหาได้ทุกสิ่งที่คุณต้องการที่นี่ ไว้วางใจและลองใช้ผลิตภัณฑ์เหล่านี้ คุณจะพบความแตกต่างอย่างมากหลังจากนั้น

แผ่นโพลีเมอร์เสริมคาร์บอนไฟเบอร์ HM-1.2T

แถบ/แผ่นลามิเนต/แผ่นโพลีเมอร์เสริมคาร์บอนไฟเบอร์ที่มีความแข็งแรงสูง (CFRP) สำหรับการเสริมความแข็งแรงโครงสร้างและการซ่อมแซมคอนกรีต

เพิ่มเติม >

HM-120CP กาวติดแผ่นคาร์บอนไฟเบอร์

กาวติดแผ่นคาร์บอนไฟเบอร์ Horse HM-120CP เป็นกาวอีพอกซี 2 ส่วนที่มีความแข็งแรงในการยึดเกาะสูง ทนทานต่อการเฉือน ทนทานต่อการเสื่อมสภาพ เป็นอีพอกซีที่ใช้ยึดแผ่นคาร์บอนไฟเบอร์เพื่อเสริมความแข็งแรงโครงสร้าง

เพิ่มเติม >

แผ่นโพลีเมอร์เสริมคาร์บอนไฟเบอร์ (CFRP) HM-1.4T

แผ่นโพลีเมอร์เสริมคาร์บอนไฟเบอร์ที่มีความแข็งแรงสูง (CFRP) สำหรับการเสริมความแข็งแรงโครงสร้างและการซ่อมแซมคอนกรีต

เพิ่มเติม >

Back
Top
Close